Anbar Journal of Engineering Science
Login
Anbar Journal of Engineering Sciences
  • Home
  • Articles & Issues
    • Latest Issue
    • All Issues
  • Authors
    • Submit Manuscript
    • Guide for Authors
    • Authorship
    • Article Processing Charges (APC)
  • Reviewers
    • Guide for Reviewers
    • Become a Reviewer
    • Reviewers of AJES
  • About
    • About Journal
    • Aims and Scope
    • Editorial Board
    • Journal Insights
    • Peer Review Process
    • Publication Ethics
    • Plagiarism
    • Allegations of Misconduct
    • Appeals and Complaints
    • Corrections and Withdrawals
    • Open Access
    • Archiving Policy
    • Journal Funding Sources
    • Announcements
    • Contact

Search Results for Mustafa A. Yousif

Article
Increasing ultimate strength of reinforced concrete slab by using Reactive Powder Concrete and study the effect of high temperature on them

Yahya S.Ali, Waleed A. Warsh, Mustafa A. Yousif

Pages: 16-26

PDF Full Text
Abstract

The main purpose of this search is to study the punching shear behavior of fourteen specimens of Reactive Powder Concrete (RPC) two-way flat plate slabs, half of these slabs have been exposed to a high temperature up to 400 C° by using an electric oven. All slabs have dimensions of (400x400x60) mm, with steel reinforcement mesh of (Ø6mm) diameter. Laboratory tests show that there is an increase in the value of First Crack Loading (FCL) and Ultimate Load (UL) by (208, and 216.67) % and a decrease in deflection by (56.85) % due using slab with complete reactive powder relative to a slap made of normal concrete. The use of the (RPC)mixture in layers in slabs gave results close to the slab which consists of full (RPC) this gives the benefit of more than the use of a slab that contains full reactive powder concrete in terms of cost, the increase was in FCL and UL by (130.8, 169.23, 102.7 and 135.135) % and a decrease in the value of deflection by (37.17, 47.64) %. The use of a partial reactive powder mixture also showed good results, and by increasing the dimensions of the RPC area, the results were better. the increase in FCL and UL by (54, 116, and 185) % and (53, 116.67, and 166.67) % and a decrease in value of deflection by (36.12, 42.4, and 50.26) % from reference slab. When slabs are subjected to high temperatures, there may be a decrease in the value of the FCL and UL and an increase in the value of deflection when compared to models not exposed to high temperature. But when compared to the reference slab with the same circumstance showed an increase in the value of the FCL and the rate ranged between (50- 200) % and the UL was the ratio ranged between (51.35-208.1) % and a decrease in the value of the deflection where the ratio ranged (21-46) %

1 - 1 of 1 items

Search Parameters

Journal Logo
Anbar Journal of Engineering Sciences

University of Anbar

  • Copyright Policy
  • Terms & Conditions
  • Privacy Policy
  • Accessibility
  • Cookie Settings
Licensing & Open Access

CC BY 4.0 Logo Licensed under CC-BY-4.0

This journal provides immediate open access to its content.

Editorial Manager Logo Elsevier Logo

Peer-review powered by Elsevier’s Editorial Manager®

       
Copyright © 2025 College of Engineering, University of Anbar. All rights reserved, including those for text and data mining, AI training, and similar technologies.